TECHNET Archives

March 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
Hinners Hans M Civ WRALC/LUGE <[log in to unmask]>
Date:
Thu, 14 Mar 2002 14:46:09 -0000
MIME-Version:
1.0
X-To:
"Marsico, James" <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Hinners Hans M Civ WRALC/LUGE <[log in to unmask]>
Parts/Attachments:
text/plain (167 lines)
Hey Jim,

Susan's got it right - if you need flat panels measure panels and if you
need flat boards you measure boards.  IPC-TM-650 2.4.22 works for either.
Somewhere in your procurement documentation you must have specified delivery
in panel form.  Did you happen to reference IPC-A-610 anywhere?

        IPC-A-610 Rev. C Section 10.6

        Acceptable - Class 1,2,3
        * Bow and twist does not cause damage during post solder
        assembly operations or end use. Consider ''Form, Fit and
        Function'' and product reliability.
        Defect - Class - 1,2,3
        * Bow and twist causes damage during post solder assembly
        operations or end use.
        Note: Bow and twist after soldering should not exceed 1.5%
        for through-hole and 0.75% for surface mount printed board
        applications

I've seen this before - panels fail but the final boards will pass.  Our
Quality Engineers would request a waiver prior to shipping or we'd scrap
them.

Hans

AC-130 Gunship Motto: "You can run but you'll only die tired."
~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~
Hans M. Hinners
Electronics Engineer
Warner Robins - Air Logistics Center (WR-ALC/LUGE)
226 Cochran Street
Robins AFB GA 31098-1622

mailto:[log in to unmask]

Com: (478) 926 - 5224
Fax:   (478) 926 - 4911
DSN Prefix: 468


-----Original Message-----
From: Marsico, James [mailto:[log in to unmask]]
Sent: Thursday, March 14, 2002 8:12 AM
To: [log in to unmask]
Subject: Re: [TN] Board Bow and Twist


Well, I got two responses with two different interpretations...

Jim Marsico
Senior Engineer
Production Engineering
EDO Electronics Systems Group
[log in to unmask] <mailto:[log in to unmask]>
631-595-5879


        -----Original Message-----
        From:   Franklin D Asbell [SMTP:[log in to unmask]]
        Sent:   Thursday, March 14, 2002 8:17 AM
        To:     TechNet E-Mail Forum.; Marsico, James
        Subject:        Re:      [TN] Board Bow and Twist

        Regarding bow/twist for arrays, prior to separation, the array is
considered
        a board and subject to the bow/twist requirements of 6012.

        At least this is how I interpret it, and apply it in my shop.

        Regards,

        Franklin D Asbell
        Network Circuits, Inc.
        Irving, Texas 75061

        ----- Original Message -----
        From: "Marsico, James" <[log in to unmask]>
        To: <[log in to unmask]>
        Sent: Thursday, March 14, 2002 6:48 AM
        Subject: [TN] Board Bow and Twist


        > I think this is a no-brainer, but here goes...  We were delivered
boards
        in
        > panel form from one of our suppliers.  At Incoming Inspection, the
panel
        was
        > rejected for excessive bow (>75% for SMT) and returned the
supplier.  The
        > supplier called me and said that even though the panel exceeded
the bow
        > requirement, the individual boards were acceptable.  When I quoted
the bow
        > and twist requirement from IPC-6012, "Panels which contain
multiple
        printed
        > boards which are assembled on the panel and later separated shall
be
        > assessed in panel form." , he said yes, you measure the individual
boards
        in
        > the panel.  I need clarification.
        > Thanks,
        > Jim Marsico
        > Senior Engineer
        > Production Engineering
        > EDO Electronics Systems Group
        > [log in to unmask] <mailto:[log in to unmask]>
        > 631-595-5879
        >
        >
--------------------------------------------------------------------------
        -------
        > Technet Mail List provided as a free service by IPC using LISTSERV
1.8d
        > To unsubscribe, send a message to [log in to unmask] with following
text in
        > the BODY (NOT the subject field): SIGNOFF Technet
        > To temporarily halt delivery of Technet send e-mail to
[log in to unmask]:
        SET Technet NOMAIL
        > To receive ONE mailing per day of all the posts: send e-mail to
        [log in to unmask]: SET Technet Digest
        > Search previous postings at: www.ipc.org > On-Line Resources &
Databases >
        E-mail Archives
        > Please visit IPC web site http://www.ipc.org/html/forum.htm for
additional
        > information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700
        ext.5315
        >
--------------------------------------------------------------------------
        -------
        >


----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2