You know it just sounds like a great place for flux entrapment and all
kinds of nasty stuff that will happen. As far as I have ever seen if you
have crimp connectors then that is what you do. As for corrosion, it
seems like he would have more with soldered wires as well as cracking
problems. I think the best place to start is at the connector
manufacturer they should give all the reasons not to solder
Carl VanWormer
<[log in to unmask] To: [log in to unmask]
OM> cc:
Sent by: Subject: [TN] Soldering crimp connectors
TechNet
<[log in to unmask]
RG>
03/13/02 02:34
PM
Please respond
to "TechNet
E-Mail
Forum.";
Please respond
to Carl
VanWormer
We have a customer who insists that we solder our crimp connectors (after
crimping). He has had corrosion problems and is convinced that this is the
best solution. Is this a good thing? Are there any downsides we should
point out to help educate him?
Carl Van Wormer
Cipher Systems
1815 NW 169th Place, Suite 5010
Beaverton, OR 97006
Phone (503)-617-7447 Fax (503)-617-6550
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|