Hi Vinit,
We dispense adhesive using Fuji GL5's, dual nozzle .3mm nozzle for 0603 and
.4mm nozzle for 0805 (internal diameter). Adhesive dot size is :- 1.5X to
2.5X where X is the nozzle internal diameter. Working towards the 2.5X for
consistency.
Steve.
-----Original Message-----
From: Vinit Verma [mailto:[log in to unmask]]
Sent: 13 March 2002 12:19
To: [log in to unmask]
Subject: [TN] Glue Dot Size
Hi All,
Has anyone ever worked with the Pump Printing Stencil for printing glue on
pre-inserted PCBs?? This stencil is developed by DEK but I'm not too sure of
how it works? Any experiences?
Also would be too kind if somebody could tell me the glue size requirement
for 0603 and 0805 components?
Thanks in advance
Regards
Vinit Verma
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
________________________________________________________________________
This e-mail has been scanned for all viruses by Star Internet. The
service is powered by MessageLabs. For more information on a proactive
anti-virus service working around the clock, around the globe, visit:
http://www.star.net.uk
________________________________________________________________________
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|