Terri,
The answer to your technical question is:
MIL-S-13949/10 (GIN) is now IPC-4101/40 [Polyimide, 200 degree C min Tg]
MIL-S-13949/10 (GIL) is now IPC-4101/41 [Polyimide, 250 degree C min Tg]
MIL-S-13949/10 (GIJ) is now IPC-4101/42 [Polyimide, 200-250 degree C Tg]
I recommend you use the IPC-4101/41 as it is most commonly available and
good stuff.
These are all standard Eglass woven. The 4101 does not differentiate
between B and C stage, hence the one slash number. Be careful when using
the Poly in today's complex surface mount, the FR4 has a better peel
strength for small SM lands and high aspect holes in small inner lands run
into tough challenges relative to etchback.
Bill Yac
-----Original Message-----
From: Houston, Terri [mailto:[log in to unmask]]
Sent: Monday, February 18, 2002 2:33 PM
To: [log in to unmask]
Subject: [TN] Mil spec translation to IPC needed
Hi folks,
I'm looking for the IPC equivalent for laminate MIL-S-13949/10 type GIN and
prepreg MIL-S13949/13 type PGI materials.
If anyone knows what these materials are currently called in the IPC specs,
it would be greatly appreciated.
Thanks,
Terri
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|