TECHNET Archives

March 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"Dan R. Johnson" <[log in to unmask]>
Date:
Sat, 2 Mar 2002 08:44:29 +0200
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Brian Ellis <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=us-ascii
From:
Brian Ellis <[log in to unmask]>
Parts/Attachments:
text/plain (28 lines)
Dan

Sal ammoniac or ammonium chloride is the active component of one of the
most active soft-soldering fluxes ever. It has no place in electronics
assembly workshops. Its use could cause horrific ionic contamination and
consequent dendrite formation, corrosion and you-name-it. Furthermore,
its fumes are highly irritating and toxic. Forget it!

Brian

> "Dan R. Johnson" wrote:
>
> Why aren't sal amoniac blocks available from electronics suppliers any
> more? I found them from a stained glass supply house but am wondering
> why Kester  et all stopped selling them. Any ideas out there?
> Dan

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2