TECHNET Archives

March 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Phil Nutting <[log in to unmask]>
Date:
Thu, 7 Mar 2002 09:43:47 +0100
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Sasha Miladinovic <[log in to unmask]>
Content-type:
text/plain; charset=iso-8859-1
Subject:
MIME-Version:
1.0
Content-transfer-encoding:
quoted-printable
From:
Sasha Miladinovic <[log in to unmask]>
Parts/Attachments:
text/plain (31 lines)
Hello Phil,

I agree with others that promote Metcal. Those are bit more expensive but
also are durable and have great performance. We use Metcal (last 4 years)
and have 60 something of those. Low maintenance costs comparing to Weller
and Hakko that we used earlier (during 15 years).
But if you have shortage of money, I could recommend the alternative that
is good compromise to Metcal and Weller. It is competitive both considering
economical and practical aspects. Check www.jbc.es and compare the
performance and price with Metcal.
My first choice would be Metcal and JBC the second.

*************************************************************************
Sasha Miladinovic - Production Engineering
Amersham Biosciences, PCB Production, Umeå
Tel:      +46 (0) 90 150 232
Fax:     +46 (0) 90 138 372
E-mail: [log in to unmask]
*************************************************************************

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2