Hi Cathy! I recommend you investigate the possibility that the plated thru
holes in your boards has breaks/voids in the copper plating - many times
blowholes/pinholes are due to the wave solder process volatilizing trapped
"stuff" in plated thru hole wall breaks. Also remember that baking will
impact the solderability of your pwbs - usually negatively. Good Luck.
Dave Hillman
Rockwell Collins
[log in to unmask]
Cathy Killen <[log in to unmask]>@ipc.org> on 02/05/2002 04:03:38 AM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
to Cathy Killen <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
To: [log in to unmask]
cc:
Subject: [TN] Baking Boards
Hi,
Is there a procedure on baking boards. Do you bake them after a certain
shelf life or do you automatically bake them? We are finding blow holes
randomly on some boards. The boards are all from the same shipment and same
date codes. If there is a procedure does it cover baking times and
temperatures etc?
Cathy Killen
Training Instructor
The information contained in the E-mail is confidential. It is intended
only
for the stated addressee(s) and access to it by any other person is
unauthorised.
The views expressed in this E-mail are those of the author, and do not
represent the views of Smtek Europe, its associates or subsidiaries, unless
otherwise expressly indicated.
Please note: It is your responsibility to scan this E-mail for viruses.
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|