Mike,
I'm missing something or have grown way to old. Why weld anything? Don't we
still float the preg with pins in slots, etc?
Misregistration is mostly caused by improper, nonhomogeneous core and preg
selections introduced as too many up books in a press opening that may or
may not be properly calibrated and is not properly managed. In a well
managed relamination process, a very predictable flow front is effected so
everything moves associatively. Therefore, without confining the dynamics of
the process, there is little misregistration.
I need to go back to school on this, I guess, or not.
MoonMan
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|