Sunny asks:
I'd like to know which type of Ion Chromatography can measure the local
dot ionic cleanliness. Anyone can tell me which company produce this
equipment?
Doug Pauls responds:
No company that I know of builds ion chromatography equipment to do spot
ionic checks. IC equipment merely analyzes extract solutions. If you want
to measure localized ion concentrations, you have to develop a localized
extraction technique. This might involve immersion of a portion of the
assembly in extract solution, or building some time of non-contaminating
enclosure around the area to be extracted. Once you can localize the
extraction, collect the solution an analyze it with the IC equipment
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------