Graham
I think the problem is that you used the mis-typed URL in Steve's first
message, and not the correction that he posted a bit later, which was to
http://www.stevezeva.homestead.com - this works for me, whilst I agree that
megago seem to have beamed in on the 'homstead' version.
Regards
Martin
********************************************
Martin Tarr
Martin Tarr Associates
1 Methven Drive
DUNFERMLINE
Fife
KY12 0AH
[log in to unmask]
01383 723989 phone
0709 233 3181 fax
07831 550192 mobile
-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]]On Behalf Of
Graham Naisbitt
Sent: 25 February 2002 10:37
To: [log in to unmask]
Subject: Re: [TN] Dendritic Growth...
Yes, me too! Please fix it Steve?
Regards Graham Naisbitt
[log in to unmask] <mailto:[log in to unmask]>
Concoat Limited
Alasan House, Albany Park
Camberley GU16 7PH - UK
www.concoat.co.uk <http://www.concoat.co.uk>
Phone: +44 1276 691100
Fax: +44 1276 691227
Mobile: +44 79 6858 2121
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of
> [log in to unmask]
> Sent: 25 February 2002 01:05
> To: [log in to unmask]
> Subject: Re: [TN] Dendritic Growth...
>
>
> Hi, Steve,
>
> Just tried looking up your site to see these beautiful dendrite pictures,
> but found you have a bully muscling in on your link. Instead of getting to
> your site I was beamed off to http://www.megago.com/l/, who then asked me
> if I wanted to make them my home page. S.. Off! I thought, but I had to
> type your site address manually to get to the pictures.
>
> Anyone else had this problem?
>
> Peter
>
>
>
>
>
> SteveZeva@AOL
> .COM To: [log in to unmask]
> Sent by: cc: (bcc: DUNCAN
> Peter/Asst Prin Engr/ST
> TechNet Aero/ST Group)
> <[log in to unmask] Subject: Re: [TN]
> Dendritic Growth...
> ORG>
>
>
> 02/23/02
> 02:49 AM
> Please
> respond to
> "TechNet
> E-Mail
> Forum.";
> Please
> respond to
> SteveZeva
>
>
>
>
>
>
> Hi Phil!
>
> The pictures are up! Go to:
>
> http://www.stevezeva.homstead.com
>
> Those are the best examples of dendritic growth as I've ever seen! Where
> did this take place? In a SIR chamber?
>
> -Steve Gregory-
>
>
> Hi Steve,
>
> Thanks for offering to post my pictures of the dendritic growth. It will
> be interesting to see what the consensus is although since I sent the
> email
> out I have been able to get my hands on the defect and take a
> close enough
>
> look to answer the question. Let's put the picture up and see what the
> responses are.
>
> Phil
>
>
>
>
>
> [This e-mail is confidential and may also be privileged. If you
> are not the
> intended recipient, please delete it and notify us immediately; you should
> not copy or use it for any purpose, nor disclose its contents to any other
> person. Thank you.]
>
> ------------------------------------------------------------------
> ---------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search previous postings at: www.ipc.org > On-Line Resources &
> Databases > E-mail Archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ------------------------------------------------------------------
> ---------------
>
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|