This question just appeared on The SMART Group's forum as well, so I can
reiterate my answer there:
I don't think these are covered by IPC standards.
Further research gets me this quote from Werner Engelmaier:
"There is no shear strength standard for solder joints, nor can there be.
If solder joints are properly wetted, they have more than ample strength
for
normal, even severe, handling and operating conditions. If they are not
properly wetted, the strength will be inadequate; because you really do not
have a solder joint. Solder joint reliability for properly wetted SJs is
not
a function of SJ strength.
The solder joint strength in pull/shear will vary with lead geometry,
solder
volume, lead metal/metallization, the way the test is done. For
50-mil-pitch
gullwings pull strength between 2000 and 5000g are typically measured."
--
:::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::
Peter Swanson Oxfordshire, England
Dynamix Technology Ltd
IPC Standards, Guidelines & Videos - Electronics Manufacturing Bookshop
[log in to unmask] http://www.dynamixtechnology.com
:::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::
-----Original Message-----
From: My Nguyen [mailto:[log in to unmask]]
Sent: 08 February 2002 1:00
To: [log in to unmask]
Subject: [TN] Component Join Shear Test
Hello Technetters,
Besides the Wire Bond Shear Test, does Jedec, or IPC,
or other any committees have any other standard Shear
Test for Component Joins.
Your advise, again, are always appreciated.
Stacy
__________________________________________________
Do You Yahoo!?
Send FREE Valentine eCards with Yahoo! Greetings!
http://greetings.yahoo.com
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|