Werner,
Thanks for the info - forgot to mention in my initial email that
through-hole solder joints are my primary concern, rather than surface mount
ones. Early testing has shown the potential for cracking/tearing of solder
joints on wire links that I am bending after soldering (not unexpected!) I
have extremely limited scope to get tooling into the area to support the
solder joints and ensure bending occurs well clear of it. It's all a messy
business and basically a product on which design-for-manufacture has gone
out to lunch...all I can do at this late stage (no major changes to the
product possible) is try to ensure that whatever steps we take in assembly
result in a sufficiently reliable product - in this case it's an emergency
lighting control so that reliability has to be good.
Regards,
Richard van Beveren
Production Engineer
NEWTRONICS PTY LTD
(Receivers and Managers Appointed)
Private Bag No. 9
122 Melrose Drive
Tullamarine 3043
Australia
Phone: +61 3 9338 5088
Fax: +61 3 9338 5022
Email: [log in to unmask]
www.newtronics.com.au
> -----Original Message-----
> From: [log in to unmask] [SMTP:[log in to unmask]]
> Sent: Tuesday, 5 February 2002 07:31
> To: [log in to unmask]
> Subject: Re: [TN] Proving the reliability of a solder joint
>
> Hi Richard,
> Yes there is--IPC-9701. For more background also IPC-SM-785.
>
> Werner Engelmaier
> Engelmaier Associates, L.C.
> Electronic Packaging, Interconnection and Reliability Consulting
> 7 Jasmine Run
> Ormond Beach, FL 32174 USA
> Phone: 904-437-8747, Fax: 904-437-8737
> E-mail: [log in to unmask], Website: www.engelmaier.com
>
> --------------------------------------------------------------------------
> -------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
> SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
> E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> --------------------------------------------------------------------------
> -------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|