Richard van Beveren,
You may want to consider the following test methods to determine solder
joint reliability:
Vibration: JESD22-B103-A Vibration, Variable Frequency
MIL-STD 883; Test Methods 2005.2, 2006.1, 2007.2
Thermal Cycling: JESD22-A104-A Temperature Cycling
MIL-STD 883; Test Method 1010.7
The big thing is to determine the environment that the assembly will
experience during its lifetime, and develop an appropriate test. For
example, in certain aerospace applications, thermal cycling is performed
from -55C to 125C. These limits might be too severe for a commercial
applications.
Hope this helps. Good Luck.
Lee Whiteman
Senior Manufacturing Engineer
E-Mail: [log in to unmask] <mailto:[log in to unmask]>
Ph: (610) 362-1200 x208
Fax: (610) 362-1290
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of Richard van Beveren
> Sent: Sunday, February 03, 2002 9:52 PM
> To: [log in to unmask]
> Subject: [TN] Proving the reliability of a solder joint
>
>
> Can anyone help with official standards that can be used to establish the
> reliability of a given solder joint / assembly method? (other than visual
> assessment)
>
> I am considering an assembly method that involves bending of auto-inserted
> wire links after soldering. I am aware that this is not a
> preferred method
> but would like to know of any recognised tests that I can perform to test
> the reliability of the solder joint "in service." Experience (and "home
> made" vibration testing of the final product) to date has shown
> little or no
> reduction in solder joint reliability but I am keen to be able to
> say, "yes,
> I have tested this assembly/joint in accordance with IEC/DIN/MIL XXX"
>
> Thanks in advance,
>
> Richard van Beveren
> Production Engineer
> NEWTRONICS PTY LTD
>
> ------------------------------------------------------------------
> ---------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search previous postings at: www.ipc.org > On-Line Resources &
> Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ------------------------------------------------------------------
> ---------------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|