TECHNET Archives

February 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Earl Moon <[log in to unmask]>
Date:
Fri, 8 Feb 2002 08:41:34 +0100
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Tegehall Per-Erik <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="ISO-8859-1"
From:
Tegehall Per-Erik <[log in to unmask]>
Parts/Attachments:
text/plain (88 lines)
I did a study for European Space Agency that was finished last year in which
we evaluated the reliability of IBM's CBGAs and CCGAs for space
applications, i.e. packages with "hard" balls and columns. One clear result
was that amount of solder paste printed on the solder lands is very critical
for the fatigue life of solder joints to CBGAs. If too little solder paste
is printed, it will result in a meagre solder fillet between the ball and
the solder land on the PCB (since the ball does not melt). If the diameter
of the solder fillet becomes less than the diameter of the ball it will
decrease the fatigue life dramatically. Meagre solder joints may also be
caused by warpage of the PCB and maybe also by some ceramic packages
(depending on their construction and thickness). So if you go for packages
with hard balls, I would recommend that you look over how you control that
the right paste volume is printed on the solder lands prior to mounting the
components.

Per-Erik Tegehall
IVF, Sweden

-----Ursprungligt meddelande-----
Från: Earl Moon [mailto:[log in to unmask]]
Skickat: den 7 februari 2002 21:41
Till: [log in to unmask]
Ämne: [TN] Ceramic CSP's and BGA's in general


Kind folks of the IPC TechNet and those not so but well informed concering
the subject issue - for me.

I have gone back and re-read all the articles and papers concerning ceramic
packages, but for CCGA's. I am, as some of you in the past, about the great
CTE mismatch between ceramic, silicon, and MLB's without constraining or
tailoring core materials.

My "frinds" at TI and IBM have been the primary players in this game. TI's
approach to solder balls is using eutectic types - I belive though not
certain in every instance. IBM talks to hard balls (90% lead) instead - in
most cases as I again believe.

I like the hard ball approach because no collapse, of course, is effected
during reflow. Therefore, more hot air is allowed to "circulate" under and
between the balls effecting a better solder joint consistently.

I am hopeful, some of you can shed some light with positive experiences with
the aformentiond parts and their solder joint acceptable initially, and long
term reliability. Realizing we have gone down this pass a few times, I hope
there is some "new" information besides the great stuff the two companies in
question provide.

As a lover of CCGA's, past and present, by IBM, I wish these parts could use
this technology. It works first and always.

Beyond this, I am hoping TI, as a major DSP device supplier, proves its
plastic BGA (super BGA or perimeter BGA - whichever) does the job. It is
said they are packaging four chips in this package style making it lower
cost and certainly more reliable due to the CTE issue.

Any input appreciated,

MoonMan

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2