Jerry:
I use the same paste and profile to build double-sided boards with no
problems.
The side with the "lighter" componets is built first.
Chris
-----Original Message-----
From: Jerry Mosur [mailto:[log in to unmask]]
Sent: Wednesday, February 13, 2002 10:09 AM
To: [log in to unmask]
Subject: [TN] Reflow Process
Hello,
As a part of our preparations to set up an internal SMD line, I would like
to get your opinion on the following topic.
What are the problems, if any, associated with reflowing the double sided
SMT board using solder paste with different melting points for top and
bottom.
Is this a fairly common process?
If not what would you recommend as a best assembly process for double sided
SMT boards?
Thanks in advance,
Jerry
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|