Morning Folks,
Ivanoe,
Billboarding is described in IPC-A-610C on page 12-77. Figure 12-130
shows a picture of Billboarding and is acceptable for Class 1 & 2
products providing it meets the criteria stipulated.
Barry Gallegos
-----Original Message-----
From: Ivanoe Pedruzzi [mailto:[log in to unmask]]
Sent: Friday, February 22, 2002 12:11 AM
To: [log in to unmask]
Subject: Re: [TN] Defects terminology
No doubt,
Manhattan has the same meaning as tombstone. As I had lots of them I had to
learn that terminology.
Ivan Pedruzzi
Manufacturing Engineering
Jabil Circuit Italy
-----Original Message-----
From: Sklenar Vit (RBAU-EB/MGE4) [mailto:[log in to unmask]]
Sent: Friday, February 22, 2002 1:24 AM
To: [log in to unmask]
Subject: [TN] Defects terminology
Good day,
Did you come across with these defect terms - Manhattan and
Billboard ? If yes do you know what is the meaning?
I assume that Manhattan means either a lot of tombstoned parts on
PCB , right up.
Billboard?
Please can you explain the meaning ?
Thank you
Regards
Vit Sklenar MGE4VS
T: (61 3)9541 7734 F: (61 3) 9541 3909
e-mail work: [log in to unmask]
e-mail home: [log in to unmask]
> Robert Bosch (Aust) ,
1555 cnr.Centre and McNaugton Road,
> Clayton , VIC 3169, Australia
>
>
> -----Original Message-----
> From: Earl Moon [SMTP:[log in to unmask]]
> Sent: Tuesday, February 05, 2002 7:53 AM
> To: [log in to unmask]
> Subject: Re: [TN] Proving the reliability of a solder joint
>
> My company just got a copy on CD. Werner is the chair for the committee.
> Who
> else indeed? Other names read like a who's who or Hall Of Fame.
>
> Can't wait to get into this little baby!
>
> MoonCaveMan
>
> --------------------------------------------------------------------------
> -------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
> SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
> E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> --------------------------------------------------------------------------
> -------
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|