I assume that CCA stands for Conformally Coated Assembly. If so what
chemical family did the coating
fall into (acrylic, urethane, etc...)
*Usually, CCA stands for circuit card assembly, a synonym of printed wiring
assembly.
How long was this device "in the field" and how much exposure did it
receive to humidity above 80%?
*I seriously doubt this information would be recorded or known. Most units
don't come with build in humidity loggers.
BTW those "faint carbon tracks" are usually all that left when the dendrite
vaporizes due to current
flow.
*Sometimes. They can also be residual tin and lead of the dendrite
themselves.
Doug Pauls
Rockwell Collins
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------