Hi, Steve,
Just tried looking up your site to see these beautiful dendrite pictures,
but found you have a bully muscling in on your link. Instead of getting to
your site I was beamed off to http://www.megago.com/l/, who then asked me
if I wanted to make them my home page. S.. Off! I thought, but I had to
type your site address manually to get to the pictures.
Anyone else had this problem?
Peter
SteveZeva@AOL
.COM To: [log in to unmask]
Sent by: cc: (bcc: DUNCAN Peter/Asst Prin Engr/ST
TechNet Aero/ST Group)
<[log in to unmask] Subject: Re: [TN] Dendritic Growth...
ORG>
02/23/02
02:49 AM
Please
respond to
"TechNet
E-Mail
Forum.";
Please
respond to
SteveZeva
Hi Phil!
The pictures are up! Go to:
http://www.stevezeva.homstead.com
Those are the best examples of dendritic growth as I've ever seen! Where
did this take place? In a SIR chamber?
-Steve Gregory-
Hi Steve,
Thanks for offering to post my pictures of the dendritic growth. It will
be interesting to see what the consensus is although since I sent the
email
out I have been able to get my hands on the defect and take a close enough
look to answer the question. Let's put the picture up and see what the
responses are.
Phil
[This e-mail is confidential and may also be privileged. If you are not the
intended recipient, please delete it and notify us immediately; you should
not copy or use it for any purpose, nor disclose its contents to any other
person. Thank you.]
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|