To all,
I have a test board, that is gold over nickel, and .200 thick.
The problem I have is that the holes for the compliant pins should
have been drill at .045, and plated down to .040. The holes however
have finished at .045. (hole count is 1456)
The range that the assembly house can live with is .040 +/-.003.
I would have to somehow replate the barrels of the holes
with a minimum of .001-.002 mils to get within the compliant pin spec.
Soldering the pins in, is not an option.
If anyone has seen this problem before, could you please respond ASAP, with
any possible solutions, or the name of someone who might be able to fix
these boards.
Thank you,
Loren Hendrix
Sr. Designer
Limat Graphics
128 E.Liberty St.
Danbury, CT 06810
voice 203-798-9771 Ext. 218
fax 203-790-5666
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|