Beat me to it! If you do a lot of this or the wire is very thin, you may
want to look at a lower tin content solder, also put some good extraction
over the pot.
Kind Regards
Mike Fenner
Applications Engineer, European Operations
Indium Corporation
T: + 44 1908 580 400
M: + 44 7810 526 317
F: + 44 1908 580 411
E: [log in to unmask]
W: www.indium.com
Leadfree: www.Pb-Free.com
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Sauer, Steven T.
Sent: Thursday, February 21, 2002 8:23 PM
To: [log in to unmask]
Subject: Re: [TN] stripping insulation from polyu-nylon coated magnet
wire
Phil,
The simplest method is to dip the wire in a solder pot (~500°F, 260°C).
This removes the coating and tins the wire at the same time. Most
polyurethanes and nylon coatings are in thermal classes of 105°C, 130°C,
155°C and 180°C which should be removable while immersed in molten solder.
The dwell time will be significantly longer than what is used to tin
temperature sensitive components.
Another method is thermal strippers.
The least favorite and hardest to control is abrasion using an exacto knife.
Steve Sauer
Manufacturing Engineer
Northrop Grumman, Xetron
-----Original Message-----
Anyone have a reliable safe method of removing the polyurethane and nylon
coating that protects magnet wire so that the wire can be used to solder as
a jumper wire. I remember using a hot chemical salt type stripping bath
many years ago but was hoping that someone has found a better way to do
this since then.
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|