TECHNET Archives

February 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Bev Christian <[log in to unmask]>
Date:
Tue, 19 Feb 2002 18:54:00 -0500
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Bev Christian <[log in to unmask]>
Parts/Attachments:
text/plain (254 lines)
Jim,
These are expensive because:
1) There are few companies that make them
2) Demand is low
3) Working with fluorine compounds usually ain't cheap.  To give you some
idea:

For making perfluoro compounds "A number of reactive metal fluorides have
been employed, including AgF2, PbF4, HgF2 and Co F3, the last being the most
useful.  The general reaction may be expressed as follows:
>CH2 + 4CoF3--->CF2 + 4CoF2 + 2HF (at 110 - 400 C)

followed, in a separate stage, by
2CoF2 + F2 ---> 2CoF3 (250 - 400C)"1.

It is not economical because so much fluorine ends up as HF and there are a
whole pile of side reactions, which increase in number as you try to make
longer and longer chains (No surprise there.)

There may be newer, better ways, but you can bet there are still lots of
nasty things to have to deal with.  So unless the manufacturer wants to have
a lot of dissolved workers, everything is going to be done in high quality
nickel or Monel metal, with valves that costs thousands of dollars a piece.

1.  One of my favourite references, an oldy but a goody (shows what happens
to a hand put in conc. HF - good safety reminder) A.J. Rudge, The
Manufacture and Use of Fluorine and Its Compounds, Oxford University Press,
London, 1962.

regards,
Bev Christian
Research in Motion

-----Original Message-----
From: Jim Kittel [mailto:[log in to unmask]]
Sent: February 19, 2002 9:37 AM
To: [log in to unmask]
Subject: Re: [TN] Antw: [TN] Vapor Phase Soldering ReVisited!


That would certainly make VP more palatable.  If not due to VOC taxes, why
are the fluids so expensive?
Jim Kittel

-----Original Message-----
From: James TerVeen [mailto:[log in to unmask]]
Sent: Tuesday, February 19, 2002 6:08 AM
To: [log in to unmask]
Subject: Re: [TN] Antw: [TN] Vapor Phase Soldering ReVisited!


I do not think these are ozone depleter but they are very costly.

 This is the statement that they give regarding there material
 in the data you are talking about.












 Hence, Fomblin and Galden perfluoropolyether fluids have a ZERO
 Ozone Depletion Potential and are not classified as VOCs by the
 EPA.









                    Brian Ellis

                    <b_ellis@PROTO       To:     [log in to unmask]

                    NIQUE.COM>           cc:

                    Sent by:             Subject:     Re: [TN] Antw: [TN]
Vapor Phase
                    TechNet               Soldering ReVisited!

                    <[log in to unmask]

                    RG>





                    02/16/02 03:01

                    AM

                    Please respond

                    to "TechNet

                    E-Mail

                    Forum.";

                    Please respond

                    to Brian Ellis









Guenter

See http://www.ausimont.com/docs/gald_vapor.html
This gives you details of fluids with BPs of 155, 166, 200, 210, 215,
230, 240 and 260 °C. Surely you can find one to suit almost any
application in that range.

However, I repeat my earlier warning that these products are horrific
global warmers and are not exactly given away with a packet of corn
flakes.

Best regards,

Brian

Guenter Grossmann wrote:
>
> Jim
>
> I believe the VP is still a good principle. However, the industrial
partner in LEADFREE that runs the VP trials told me that he has to use a
liquid with a boiling point of 270 deg.C and that there is nothing
available that boils around 230 deg.
> I had problem to believe this but also after asking again I got the same
answer.
>
> Best regards
>
> Guenter
>
> .
>
> EMPA
> Swiss Federal Institute for Materials Testing and Research
> Centre for Reliability
> Dipl. Eng. Guenter Grossmann
>
> 8600 Duebendorf
> Switzerland
>
> Phone: xx41 1 823 4279
> Fax :     xx41 1823 4054
> mail:     [log in to unmask]
>
>
----------------------------------------------------------------------------
-----

> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search previous postings at: www.ipc.org > On-Line Resources & Databases
> E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
>
----------------------------------------------------------------------------
-----


----------------------------------------------------------------------------
-----

Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----




----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2