TECHNET Archives

February 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 15 Feb 2002 10:44:26 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="US-ASCII"
From:
Parts/Attachments:
text/plain (104 lines)
Hi Graham

I would definitely be interested in purchasing a copy of the data on CD ROM.
Please provide cost and if possible a list of the topic/papers that will be
included.

best regards,

Faz,
(Dan Fazioli, Engrg Technical Mgr.
Smiths Aerospace Electronics Systems
Clearwater, Florida. 33772
727-532-6333)

____________________Reply Separator____________________
Subject:    Re: [TN] RELIABILITY DATA/INFORMATION CORRELATED TO DESIGN R
Author: Graham Naisbitt <[log in to unmask]>
Date:       2/15/2002 2:16 PM

Earl

I recently ran a seminar for the British SMART Group called: Design for
Reliability in a Lead-Free World.

We at the SMART Group are proposing to make a copy of all the presentations
on a CD for a small fee - to be decided.

If you or anyone else would wish to buy a copy, please let me know.

Regards Graham Naisbitt

[log in to unmask] <mailto:[log in to unmask]>

Concoat Limited
Alasan House, Albany Park
Camberley GU16 7PH - UK

www.concoat.co.uk <http://www.concoat.co.uk>

Phone: +44 1276 691100
Fax: +44 1276 691227
Mobile: +44 79 6858 2121


> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of Earl Moon
> Sent: 15 February 2002 11:43
> To: [log in to unmask]
> Subject: [TN] RELIABILITY DATA/INFORMATION CORRELATED TO DESIGN RULES
>
>
> Folks,
>
> Before I go down the reliability test road, using HALT/HAST, I
> would ask if
> data or information exists in industry, as IPC or other, clearly
> correlating
> design rule selections (BGA pad sizes, etc., manufacturing
> processes, etc.)
> to that data? Most large companies in this business, as you all know,
> continually develop this data and have clear evidence that if you use a
> certain design rule and introduce the design to a certain
> process, a certain
> product reliability factor will be realized.
>
> Does the IPC, through its committee work and round robin testing,
> have such
> data available? Seems like I know the answer, but may never have
> bothered to
> ask before. This data must be available as the IPC could never have
> developed its guidelines without it, right?
>
> A little fuzzy after a rather interesting night out of my cave,
>
> Moon Man
>


**********************************************************************
This e-mail and any files transmitted with it are confidential and may
be legally privileged or otherwise exempt from disclosure under
applicable law. This e-mail and its files are intended solely for
the individual or entity to whom they are addressed and their content
is the property of Smiths Aerospace.  If you are not the intended
recipient, please do not read, copy, use or disclose this communication.
If you have received this e-mail in error please notify the e-mail
administrator at [log in to unmask] and then delete this e-mail, its
files and any copies.

This footnote also confirms that this e-mail message has been scanned
for the presence of known computer viruses.
***********************************************************************

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2