Bob,
Oops, good point! That was one of the reasons we switched from GE RTV108 to Dow Corning 737 because 737 is a neutral cure and doesn't use acetic acid (that stinky foot smell) to cure. The acetic acid can do nasty things to bare copper during the cure cycle.
Let me retract my hardware store suggestion!
Phil
-----Original Message-----
From: bbarr [mailto:[log in to unmask]]
Sent: Wednesday, February 13, 2002 8:54 AM
To: [log in to unmask]
Subject: Re: [TN] Adhesive Recommendations?
Use caution if you buy a general purpose RTV at a hardware store. Many of
those products will be corrosive to electronics. If it smells like vinegar
when it cures it is no good for electronics. You must use an electronic
grade of RTV on boards. We use Dow Corning 3145 all the time for staking
with excellent results. We too transfer it to a syringe and use an EFD
dispenser.
Bob
=======================
Robert Barr
Manufacturing Engineering
Formation, Inc.
Voice: 856-234-5020 x3035
Fax: 856-234-6679
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of Phil Nutting
> Sent: Wednesday, February 13, 2002 8:15 AM
> To: [log in to unmask]
> Subject: Re: [TN] Adhesive Recommendations?
>
> For instant gratification there are several clear RTV products
> available at the local hardware store that are used for general
> bonding and sealing. Like replacing those tiles in the bathroom
> that have come loose.
>
> It isn't high tech but it has worked for many years.
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|