TECHNET Archives

February 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Bev Christian <[log in to unmask]>
Date:
Mon, 11 Feb 2002 17:30:53 -0000
Reply-To:
Subject:
From:
Mike Fenner <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (109 lines)
I think the flux guys would claim, with justification in some cases, that
their "at the point of use" kits are designed for a non chemist to be able
to use reliably. Conversely if you have a lab with proper chemists in it,
then they will be most likely able to do the titration anyway.

Kind Regards

Mike Fenner

Applications Engineer, European Operations
Indium Corporation
 T: + 44 1908 580 400
M: + 44 7810 526 317
 F: + 44 1908 580 411
 E: [log in to unmask]
W: www.indium.com
Leadfree: www.Pb-Free.com



-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Bev Christian
Sent: Monday, February 11, 2002 2:55 PM
To: [log in to unmask]
Subject: Re: [TN] Flux Testing using Titration


Neil,
It depends on who you ask.  If you are talking about the quick and dirty
at-the-wave-solder-machine titrations, I doubt they will recommend you use
anything but their kits.  But if you are going to do it in a lab with proper
equipment, trained personnel, you may be able to nicely ask them for their
lab procedure on how they do it.  Some of them will give it to you, and some
won't.

regards,
Bev Christian
Research in Motion

-----Original Message-----
From: Atkinson, Neil [mailto:[log in to unmask]]
Sent: February 11, 2002 7:25 AM
To: [log in to unmask]
Subject: [TN] Flux Testing using Titration


We are currently buying titration kits from a solder / flux supplier.  Does
anyone out there buy the chemicals to do this from a standard chemical
supplier (cheaper?) and if so which chemicals do I need, in what
concentrations etc and can I just follow the same procedure and use the flux
manufacturer's titration curves?

Thanks,

Neil


________________________________________________________________________
This e-mail has been scanned for all viruses by Star Internet. The
service is powered by MessageLabs. For more information on a proactive
anti-virus service working around the clock, around the globe, visit:
http://www.star.net.uk
________________________________________________________________________

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2