Yor supplier can be more specific that we can. For example, one supplier
says the specific gravity is:
Low Solids No-Clean||Rosin Free Low Solids No-Clean||VOC-Free
No-Clean||VOC-Free No-Clean
0.800 ± 0.005||0.814 ± 0.003||1.014 ± 0.010||1.008 ± 0.003
Dave Fish
----- Original Message -----
From: "Prasad An" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, February 07, 2002 7:59 AM
Subject: [TN]
> Hi all
>
> Can any one tell me how to measure the Specific Gravity of NO-CLEAN FLUX..
>
>
>
> PRASAD
>
> --------------------------------------------------------------------------
-------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> --------------------------------------------------------------------------
-------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|