Hi Olivia,
You should be very happy if your inspection people catch more than 50% of the defects. The remainder will simply be overlooked. This is not an opinion, but it's a proven fact !!
It is just not possible to inspect quality into the product, instead you should focus on the assembly process.
B.T.W. on my website I have some nice software available (it's a free beta version) that may be helpfull for you with the inspection of the pcb's after pick&place machine. The URL is http://www.smtinfo.net/smtmaestro/smtmaestro.html
Daan Terstegge
SMT Centre
Thales Communications
Unclassified mail
>>> Olivia Mc Dermott <[log in to unmask]> 01/03 4:01 pm >>>
We do have inspection points throughout the process. The problem is they are
also missing defects and letting them through to final inspection.I wondered
if there is a direct instruction on inspecting.
1. you do this
2. you do this.
>From: Kathy Kuhlow <[log in to unmask]>
>Reply-To: "TechNet E-Mail Forum." <[log in to unmask]>
>To: [log in to unmask]
>Subject: Re: [TN] Final Audit/Inspection
>Date: Thu, 3 Jan 2002 08:49:32 -0600
>
>I would first start with some in-process sampling so you can pinpoint what
>types of defects the process is currently producing. Do you see more
>missing components from surface mount or do you have a problem withe solder
>shorts on the solder side because of wave issues or snapping problems.
>All to many organizations use a final inspection as a safety net. In my
>dream world I would have no one doing final inspection but bring it back to
>the process and do the inspection at the process through auditing by both
>production and quality personnel so immediate feedback can be accomplished.
> Otherwise you get data that is out of date and you can't really take
>effective corrective actions, especially if your world is as a CM or small
>run lots.
>
>If you must do a final inspection then we typically start with a complete
>part verification (value, polarity, AVL check) than solder (quality,
>quantity, lead placement) and finally any specific customer
>instructions(labeling, rev add, etc).
>
>Kathy
><< TEXT.htm >>
_________________________________________________________________
Send and receive Hotmail on your mobile device: http://mobile.msn.com
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|