Jeffrey
I don't have data to back up this statement, but IMO the discoloration is
has a time variable also. Back in the old days, I've seen double sided FR-4
start to brown after two or three hours at 175 C.
Don Vischulis
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Guy Ramsey
Sent: Thursday, January 17, 2002 12:23 PM
To: [log in to unmask]
Subject: Re: [TN] Scorching Temp for FR4
My experience has been that they start to discolor around 260°C. I'm sure
this varies. The board will be charcol by 350°.
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of McGlaughlin, Jeffrey
> A
> Sent: Thursday, January 17, 2002 1:06 PM
> To: [log in to unmask]
> Subject: [TN] Scorching Temp for FR4
>
>
> Tech-sters
>
> Does anyone know of a reference that gives approximate temperatures for
> discoloration (scorching) of FR4 material?
> We have a scorched board and would like a ballpark figure on how
> hot it was
> before failure.
>
> Jeffrey A. McGlaughlin CID
> Sr. Designer
> Battelle Memorial Institute
> Columbus Ohio
> [log in to unmask]
>
> ------------------------------------------------------------------
> ---------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search previous postings at: www.ipc.org > On-Line Resources &
> Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ------------------------------------------------------------------
> ---------------
>
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|