Hi Phil, if I remember correctly Arconium Specialty alloys is in Rhode
Island and was bought by Alpha, perhaps if you call Walter Zelop at Alpha he
should be able to help you out.

Till later, Leo Lambert.
EPTAC Corp
[log in to unmask]

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of David Hillman
Sent: Friday, January 11, 2002 3:48 PM
To: [log in to unmask]
Subject: Re: [TN] Solder properties


Hi Phil! Ostalloy is an alloy designation for the Arconium Specialty Alloys
company. But - I can't find any listing for an alloy 428 on my Arconium
alloy data sheets. You might try contacting Arconium directly
(arconium.com) for information. Good Luck.

Dave Hillman
Rockwell Collins
[log in to unmask]




Phil Hinton <[log in to unmask]>@ipc.org> on 01/11/2002 02:07:31 PM

Please respond to "TechNet E-Mail Forum." <[log in to unmask]>

Sent by:  TechNet <[log in to unmask]>


To:   [log in to unmask]
cc:

Subject:  [TN] Solder properties


Could anyone give me the properties of a solder, Ostaloy 428 (ie) MP,
Solidus, liquidus, composition.

Phil Hinton


----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To recieve ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To recieve ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2