Subject: | |
From: | |
Reply To: | (Leadfree Electronics Assembly Forum) |
Date: | Mon, 7 Jan 2002 15:33:04 -0000 |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
I have a rather old, but I believe still up to date list of toxins and
furanes given off by burning FR4 resin systems based on TBBA-EP /
Dicyaniamide. The list was compiled during Thermolysis Studies with
Brominated Epoxy Resins at various temperatures by Dr. Kugler Ciba-Geigy AG
(presented at EIPC Zurich 1987). I'd be happy to forward this on to any
interested parties. Please mail me off-line.
Colin McVean
Polyclad Technologies
---- Original Message -----
From: "David Bergman" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Monday, January 07, 2002 2:32 PM
Subject: Re: [LF] Matsushita Succeeds in Recycling Solder Residue
UsingSesame Seeds
> Hi Karsten
>
> Regarding #3 - I have not be able to find studies pointing to dioxins and
furans associated with flame retardants in PCB scrap. TBBPA is not supposed
to have this problem. Though I do know it is seen with other flame
retardants. Do you any details?
<snip>
---------------------------------------------------------------------------------
Leadfee Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|