Mike Sewell Suggests: Would microabrasive blasting of the coating be an
alternative to chemical stripping?
*Just be aware that microabrasive blasting generates a hell of a static
charge. Enough to kill a static sensitive component. I think the EMPF did
some work in microabrasion methods relative to ESD in the late 80s early
90s. Check with the librarian at www.empf.org.
Doug Pauls
Rockwell Collins
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------