TECHNET Archives

January 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Earl Moon <[log in to unmask]>
Date:
Wed, 30 Jan 2002 15:56:16 -0800
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, David Fish <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="iso-8859-1"
From:
David Fish <[log in to unmask]>
Parts/Attachments:
text/plain (71 lines)
This component package is a pain in a spot somewhat below the neck, because
of the slug of metal used for a heat sink in the package. Issues are:
* Process measurement needs to be measured on the solder balls [both at the
inner row and the corner]. The difference in CTE of all the elements of this
package can make it difficult to profile otherwise.
* Process verfication with a common xray machine is close to futile.

Further, in these TI DSP, Dr. Cemel Basaran, SUNY Buffalo, 716-645-2114
X2429, [log in to unmask] has seen:
* Thinner [2 micron] than normal [20-micron ] AuSn4 IMC
* Black pad

Dave Fish



----- Original Message -----
From: "Earl Moon" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, January 30, 2002 10:48 AM
Subject: [TN] CSP/DSP SOLDERING PROBLEM?


> Folks,
>
> Have some CSP's that are TI DSP's (320c6203 TMX 320C6203 BGLS), or some
such
> thing. I can't imagine there being solderability issues with these things,
> but then I didn't think I'd live this long. However, after examining all
> other possible process variables, and resolving them to some extent, these
> things look to be the last straw.
>
> Solder joints on these parts, mostly, aren't. The "C" clamp thing picture
is
> holding one of the critters on the board to make electrons flow.
>
> Does anyone have any issues with these parts and their solderability? I do
> appreciate the assistance. Steve, these probably are coming your way.
>
> Earl
>
> --------------------------------------------------------------------------
-------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> --------------------------------------------------------------------------
-------
>

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2