I found an old copy of ipc-tp-1115 "Selection and Implementation Strategy for A
low-residue no-clean process" published Dec. 1998. Have not read thru it yet
but also have simular interest in implementation of no-clean. If any one has
more referance info i would appreciate.
[log in to unmask] on 01/30/2002 09:05:36 AM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond to
[log in to unmask]
To: [log in to unmask]
cc: (bcc: Warren Crow/US/I-O INC)
Subject: Re: [TN] Flux residue with a no-clean process
Hi Kathy,
I am very interested in this as we have the following processes:
1. No clean smt - no clean wave solder - saponified wash
2. No clean smt - clean wave solder - aqueous wash.
Could you please advise why this would be detrimental. Would this affect the
reliability of the joints and if so is there a paper on this.
Thanks for your help.
Best regards
Marc.
-----Original Message-----
From: Kathy Kuhlow [mailto:[log in to unmask]]
Sent: Wednesday, January 30, 2002 2:20 PM
To: [log in to unmask]
Subject: Re: [TN] Flux residue with a no-clean process
<< File: TEXT.htm >> IPC-610 has no-clean residues as acceptable. Is it
possible that flux may have been mixed with a washable? Washing a no-clean
off is more detrimental than leaving it alone.
Is the assembly conformally coated? Is the application intended to be in a
wet or high humidity/moisture enviroment?
Kathy
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|