TECHNET Archives

January 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Date:
Mon, 28 Jan 2002 09:06:39 +0000
Reply-To:
Roger Bilham <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Type:
text/plain;charset=iso-8859-1
In-Reply-To:
Content-Transfer-Encoding:
8bit
From:
Roger Bilham <[log in to unmask]>
Parts/Attachments:
text/plain (43 lines)
Phil

I believe that Soldertec http://www.lead-free.org keeps a directory of
lead free products, which may help you.

Patents covering the composition you give have been applied for by
Matsushita, Sony and Siegfried Pfyffer (and probably others by now), who
may be able to supply information.

Have fun.
Roger Bilham

In article <[log in to unmask]>, [log in to unmask] writes
>    Hi
>
>    Since I did not get any answers to my earlier inquiry after all of
>    the smart guys have returned from Apex.
>
>    Does any one have a supplier source for a solder,
>    Sn96.3/Ag2.5/Cu0.7/Zn 0.5
>
>    Thanks
>
>    Phil Hinton

--
Roger Bilham
Roger Bilham Consultancy
Tel: +44 (0)20 8467 8819
Fax: +44 (0)8700 548 613
Mobile +44 (0)7 941 122 446

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2