Phil
I have a source for SnZn9 and Sn ZnBi ( don't know the composition right now) where we get the stuff for research:
Showa Denko
489 fifth Avenue 18th floor
New York, NY 10017
Phone: 1-212-370-0033
Fax: 1-212-370-4566
or in Japan:
13-9 Shiba Daimon 1-Chome
Minato- ku
Tokyo 105-8518
Solder is pretty cheap. However shipping from Japan costs an arm and a leg.
Have a great day
Guenter
.
EMPA
Swiss Federal Institute for Materials Testing and Research
Centre for Reliability
Dipl. Eng. Guenter Grossmann
8600 Duebendorf
Switzerland
Phone: xx41 1 823 4279
Fax : xx41 1823 4054
mail: [log in to unmask]
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------