Hi Stacy,
First, get your self a copy of IPC-7530 "Guidelines for Temperature Profiling
for Mass Soldering Processes (Reflow & Wave)."
Second, part of your problem is the sloppy language that is being used in our
industry.
What you are referring to as "reflow profiles" are actually "oven recipes." A
given 'oven recipe' on a given machine will result in many differrent 'reflow
profiles' at the solder joints of components with different thermal masses
and construction. You definitely want to have a 'reflow profile' for each
assembly code based on the component in the assembly with the solder joints
heating up the slowest. To achieve this 'reflow profile' for a code may
require a different 'oven recipes' for each of your reflow ovens--you will
know this only after monitoring the 'profiles' resulting from a given
'recipe' for these diffent codes.
Third, the number of your 'recipes' sure does sound excessive.
Fourth, "above 183: 40-80 sec" is irrelevant. You need to be at least about 5
seconds above (Liquidus for you solder + 25°C) [that is 208°C for eutectic
Sn/Pb] for any solder joint in your assembly to assure proper wetting on a
consistent basis.
Fifth, remember, the object of the whole excercise is to make sure ALL solder
joints in an assembly receive adequate heat during reflow.
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL 32174 USA
Phone: 904-437-8747, Fax: 904-437-8737
E-mail: [log in to unmask], Website: www.engelmaier.com
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|