TECHNET Archives

January 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
7bit
Sender:
Subject:
From:
Stephen Gregory <[log in to unmask]>
Date:
Tue, 15 Jan 2002 21:10:31 EST
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (44 lines)
Hi All!

Another weird one again, I'll post a picture tomorrow when I get back into
work. But a preface to the picture, is that we built a board that was wave
soldered, and after post wave cleaning, you could see a faint outline of
where masking was applied over holes, we use water soluble dots over holes
etc...I've seen that before, but it usually isn't so noticable that it's a
big deal.

However, on this particular board we're doing some jumper wires that go from
the bottomside up to the top, this is done after wave and everything else.
The operators soldered the wires to where they needed to go, and then needed
to clean the boards prior to tak-pak'ing them to the board. So before sending
them to the cleaner, they used kapton tape to secure the wires to the board
so they didn't flop around in the cleaner...makes good sense to me. When they
got the boards back outta the cleaner and removed the tape, there were all
these dark spots in the mask beneath where the tape was...it looks kinda'
bad. But the mask is intact as far as I can see, there is no degradation at
all...it just looks bad...almost looks like something deeper, but I'm sure
it's just mask discoloration...

I baked the boards to see if that would change anything, but it didn't. The
mask is a LPI, don't know the brand. I'll post a picture tomorrow morning.
But have you ever run across LPI masks lightening or darkening, showing
outlines of masking materials after wave soldering, or cleaning (kapton
tapes, preformed dots, etc..)?

What causes that?

Thanks everybody!

-Steve Gregory-

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2