Technetters,
My company is having a solder ball problem on the wave solder. The
issue is primarily caused by overly large un-masked vias on both sides. The
via diameter is 25 mils with an annular ring of 25 mils on a .062" board.
On the wave solder process, the flux gets entrapped inside the vias and no
matter what we do on the pre-heating section there still flux remaining
inside that causes the solder to explode into tiny solder balls when it gets
to the laminar section of the wave, like a volcano effect on the component
side. These boards have also a good amount of the same vias under fine pitch
QFP devices , this narrows our process window if we want to heat the board
even more. Heating the board more on the preheaters to resolve the solder
ball problem leads on re-reflowing of the leads of those devices and quality
problems as a result of that, the QFP pins pop up and become un-soldered.
The customer does not want to use smaller vias or get them masked off since
vias are used for test and rework purposes, they want to be able to insert
wires inside the vias in case they need to change the board configuration.
Any ideas on what to do with the wave process to resolve this issue?
Any ideas would be greatly appreciated.
Jorge Rodriguez
Process Engineer
Varian Electronics Manufacturing
615 South River Drive
Tempe, AZ 85281
Phone: (480) 968-6790 X 4258
Fax: (480) 829-4000
E-mail: [log in to unmask]
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To recieve ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|