TECHNET Archives

January 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Date:
Wed, 9 Jan 2002 09:17:20 -0800
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
From:
Mel Parrish <[log in to unmask]>
Parts/Attachments:
text/plain (135 lines)
Lou,
Think we addressed this in the initial meetings for 610D.  For the purpose
of the Amendment, we wanted to have a defect statement for the stand alone
acceptable condition in the 610C, paragraph 10.4.
For those concerned about frequent changes, consider that the last revision
took over three years to complete. So don't hold your breath or get too
concerned just yet.
Best regards,
Mel

It's a beautiful day in ALABAMA!

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Lou Hart
Sent: Wednesday, January 09, 2002 6:42 AM
To: [log in to unmask]
Subject: Re: [TN] Lead Length/Protrusion


Mel, can I suggest removing 10.4 from 610 entirely.  It deals with solder
mask, not laminate.  The "defect" added in amendment 1 is redundant with
portions of section 9.  Lou Hart

-----Original Message-----
From:   Mel Parrish [SMTP:[log in to unmask]]
Sent:   Wednesday, January 09, 2002 11:05 AM
To:     [log in to unmask]
Subject:        Re: [TN] Lead Length/Protrusion

Olivia
Amendment 1 to 610C identifies 2.5mm as the correct value.  The amendment
was released a couple of months ago and is available on the IPC web site.
By the way, work is in progress toward Revision D to this document.  We
have
accumulated a number of comments and would appreciate any additional
information that you would like to see in the new 610. We certainly could
use some additional information on the newer technology applications.

The next technical meeting will be at APEX on 19 Jan.

Mel Parrish
Soldering Technology International
Madison, AL
256 705 5530
256 705 5538 Fax
[log in to unmask]




-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Olivia Mc Dermott
Sent: Wednesday, January 09, 2002 5:41 AM
To: [log in to unmask]
Subject: [TN] Lead Length/Protrusion


Hi ALl,
Why are there 2 references to lead length/protrusion in IPC-A-610C. In
'Component Installation Location/Orientation' - point 5.2.7.1 table 5.2
lead
protrusion for class 2 is 2.5mm but in 'Soldering' point 6.2 table 6.1 lead
protrusion for class 2 is 2.3mm. Which one do we use?

_________________________________________________________________
MSN Photos is the easiest way to share and print your photos:
http://photos.msn.com/support/worldwide.aspx

------------------------------------------------------------------------
----
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
SET
Technet NOMAIL
To recieve ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
------------------------------------------------------------------------
----
-----

------------------------------------------------------------------------
---------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
SET Technet NOMAIL
To recieve ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
------------------------------------------------------------------------
---------

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To recieve ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To recieve ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2