TECHNET Archives

January 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
"<Peter George Duncan>" <[log in to unmask]>
Date:
Wed, 9 Jan 2002 13:01:55 +0800
Content-type:
text/plain; charset=us-ascii
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Parts/Attachments:
text/plain (175 lines)
It did us well enough in Marconi for a while, but took a bit longer to cure
(or something) than alternatives. We changed to Eccobond 45 eventually.

Peter Duncan




                    "Bissonnette,
                    Jean-Francois"         To:     [log in to unmask]
                    <JBissonnette@W        cc:     (bcc: DUNCAN Peter/Asst Prin Engr/ST
                    ABTEC.COM>             Aero/ST Group)
                    Sent by:               Subject:     Re: [TN] Staking compounds
                    TechNet
                    <[log in to unmask]
                    G>


                    01/08/02 10:56
                    PM
                    Please respond
                    to "TechNet
                    E-Mail Forum."






Since we're in that subject, anyone has a good or bad opinion on loctite
444 (Tack pack).  We sometimes use it for staking wire
to pcb.

Thanks!

JF
     -----Original Message-----
     From: Hinners Hans M Civ WRALC/LUGE
     [mailto:[log in to unmask]]
     Sent: Tuesday, January 08, 2002 9:44 AM
     To: [log in to unmask]
     Subject: Re: [TN] Staking compounds

     Hi All,

     This is great information.  I've had an Assembly supplier suggest
     using an RTV to stake discrete components to FR-4.  Graham confirmed
     that it wasn't a good combination with a silicone based conformal
     coating.  (Thanks Graham.)  The last thing I or the customer needs is
     dewetting of the conformal coating.  My applications are hi-rel
     military avionics - in a rather harsh environment: high vibration,
     high humidity and some salt water.

     Is there some cutoff point when it's better to go with mechanical
     staking?  I'm new to staking.

     Hans



     Integrity First  -  Service Before Self  -  Excellence in All We Do
     ~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~
     Hans M. Hinners
     Electronics Engineer
     Warner Robins - Air Logistics Center (WR-ALC/LUGE)
     226 Cochran Street
     Robins AFB GA 31098-1622

     mailto:[log in to unmask]

     Com: (478) 926 - 5224
     Fax:   (478) 926 - 4911
     DSN Prefix: 468


          -----Original Message-----
          From: Dieselberg, Ron [mailto:[log in to unmask]]
          Sent: Tuesday, January 08, 2002 7:28 AM
          To: [log in to unmask]
          Subject: Re: [TN] Staking compounds



          Doug, we have used CONAP K-20 for a long time with good results.
          We have also used Loctite 416 with 18580 activator. The Loctite
          is easier to use since it "sets" more quickly.


          All depends on how you want to use it and how much time you have
          available for curing.
          In either case be sure the materials that you are going to stake
          to are "sqweekey" clean!


          Ron Dieselberg
          Trainer/Auditor
          CMC ELECTRONICS
          CINCINNATI
          [log in to unmask]


                    -----Original Message-----
                    From:   [log in to unmask] [
                    mailto:[log in to unmask]]
                    Sent:   Monday, January 07, 2002 14:41 PM
                    To:     [log in to unmask]
                    Subject:        [TN] Staking compounds


                    Good day all,


                    I am curious as to what all y'all use for staking
                    compounds (to fix wires
                    or components in place) on your assemblies, especially
                    if you are in the
                    high-rel area or aerospace sector.  Thanks.


                    Doug Pauls
                    Rockwell Collins


                    ---------------------------------------------------------------------------------

                    Technet Mail List provided as a free service by IPC
                    using LISTSERV 1.8d
                    To unsubscribe, send a message to [log in to unmask] with
                    following text in
                    the BODY (NOT the subject field): SIGNOFF Technet
                    To temporarily halt delivery of Technet send e-mail to
                    [log in to unmask]: SET Technet NOMAIL
                    To recieve ONE mailing per day of all the posts: send
                    e-mail to [log in to unmask]: SET Technet Digest
                    Search previous postings at: www.ipc.org > On-Line
                    Resources & Databases > E-mail Archives
                    Please visit IPC web site (
                    http://www.ipc.org/html/forum.htm) for additional
                    information, or contact Keach Sasamori at
                    [log in to unmask] or 847-509-9700 ext.5315
                    ---------------------------------------------------------------------------------





WABTEC CORPORATION CONFIDENTIALITY NOTE
The content contained in this e-mail transmission is legally privileged and
confidential information intended only for the use of the individual or
entity named herein. If the reader of this transmission is not the intended
recipient, you are hereby notified that any dissemination, distribution, or
copying of this transmission is strictly prohibited.







[This e-mail is confidential and may also be privileged. If you are not the
intended recipient, please delete it and notify us immediately; you should
not copy or use it for any purpose, nor disclose its contents to any other
person. Thank you.]

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To recieve ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2