Use baskets. I'll let Steve Z. or Moonman jump in since I can't remember who makes 'em.
Jason Gregory
Software Specialist - NPI Group
SCI Systems/Plant 2
13000 S. Memorial Pkwy.
Huntsville, AL. 35803
(256) 882-4107 x3728
[log in to unmask]
>>> Mark Charlton <[log in to unmask]> 12/05/01 10:31AM >>>
We're experiencing some damage to some small PCB's (0.75"x1.75") that
occurs during their trip through the aqueous cleaner. The boards are
originally processed in a panel but some require rework or additional
processing once they have been depanelized.
Can anyone suggest a method to secure these small boards inside the wash
racks as to prevent this damage?
Mark Charlton
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------