Hi Dave,
You write:
>As a self-described proponent of flux only mounting of BGA, please help us
>understand the impact on product reliability of reduced solder in these
connections.
I am with the  Moonman on this. SJ reliability is affected by solder joint
height, not very much by solder volume. In fact, data show that
'hour-glass'-shaped SJs have slightly greater reliabiliity than
'barrel'-shaped ones.

Werner Engelmaier

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2