Unfortunately the customer does not accept even the 2mm allowed by IPC for
a straight drop in radial part. RTV was also rejected.
The bottom of the cap does have a flexible rubber seal on the bottom that
takes some of the stress. The part can be "pushed" into the PTH but it does
do a number on the plating of the lead and the barrel.
What I am down to now I think is a Liability/Reliability issue.
---------------------------------------------------------------------------------