Hello,
Thanks in advance if you have taken the time to read this!

#1- Im trying different materials in a spray application. Both are cured
using UV. One material does a "secondary cure" w/ moisture. This is cool
because after 100 hours after UV cure, all material is fully cured.
The other material Im trying uses HEAT for a secondary cure, or, if
shodowed during UV cure, the material wont cure and never will. Obviously I
dont want the stuff dripping or running anywhere, but being new to this
wonderful process, just dont feel good about leaving uncured material on a
product for it's entire life. Iv been told that you can "test" the product
to see if the uncured material is causing a problem but Im not sure what
type of test that would consist of. Any insight?

#2- Has anyone out there ever installed refelctive metal plates in their UV
oven to limit shadowing?

Thanks so much,

Mike Manwell

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2