The sulphur content probably is the source or the 'smell'... like rotten
eggs.
- Bill Brooks
-----Original Message-----
From: Charles Caswell [mailto:[log in to unmask]]
Sent: Friday, December 14, 2001 11:17 AM
To: [log in to unmask]
Subject: Re: [TN] Alumina filled Polysulfide compound...
Steve, I am at home so I don't have the info here . We use the same
stuff to bond components on some boards. I don't think you will find the
stuff already mixed with the AlO2. I couldn't. The polysulfide IS fuel
tank sealant. We mix it in small batches with approx. equal parts of
AlO2 and the base material by weight. I wonder if we have the same
customer. I will try to get into work tommorow and send some info, if
not then on Mon. By the way, the stuff stinks.
Charles Caswell
Process Lead, PCB
Frontier Electronic Systems
-----Original Message-----
From: Stephen R. Gregory
Sent: Fri 12/14/2001 8:26 AM
To: [log in to unmask]
Cc:
Subject: [TN] Alumina filled Polysulfide compound...
Hi All!!
...tappity-tappity-tappity...(doin' my thank gawd it's Friday
dance! hehehe)
I was wondering if someone could point me in a direction where I
could find some alumina filled polysulfide compound, per MIL-S-8802,
class A-2, with 50 plus or minus 10%, 325 mesh aluminum oxide powder...
This is something that is called out on a drawing for a board
that's using this material to strain relief two small battery cables
that are installed on the board...I've searched and find a bunch of
stuff about polysulfide compounds, but nothing alumina filled. If I
search under MIL-S-8802, I find all kinds of polysulfide sealers for jet
fuel tanks, but still nothing alumina filled...
Any help will be much appreciated
-Steve Gregory-
M!ꭝLj)Kiخu龁Zy퉪y<+బx
!$uᰭ{.n+ᰉzwZ,j뭠M!T9褰_ଢYh)牼m{ax崃`ӓr톏zWR
cNTr:-zjh(Z˖^搖+ޯ*M!莝lzwmZ0x&zঁM7Ⲝw4 ഞj!-x,j0탔*\y
zڱ!>W횱
+H<,nȭzm쵩rf顶g譧]بb+bz+r␉i蒉Jy!Ij䰃((
+Î{G衱
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|