Hi Jerry,
you should look at the specs regarding the hight you reach when the deposit
is melting and becoming convex again. Does this specified hight comply with
components coplanarity tolerances ?
This made me think about this technology ...
Wolfgang
> -----Original Message-----
> From: Jerry Mosur [mailto:[log in to unmask]]
> Sent: Wednesday, December 05, 2001 10:15 PM
> To: [log in to unmask]
> Subject: [TN] SiPAD
>
>
> Greetings,
>
> Our assembly guys came across a PCB product called SiPAD. It
> is a patented
> (by Siemens) way of adding a layer of SMD paste, then curing
> and leveling it
> and finally spraying the whole board with a layer of flux. A layer of
> protective paper is applied over the entire surface so the
> flux doesn't dry
> out and stays tacky.
> The claim to fame is that it is suppose to save one
> manufacturing step,
> solder paste application.
>
> Any comments?
>
> Thanks in advance.
>
> --------------------------------------------------------------
> -------------------
> Technet Mail List provided as a free service by IPC using
> LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with
> following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following
> message: SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources
> & Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm)
> for additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> --------------------------------------------------------------
> -------------------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|