Rick, thanks for shedding more light on the subject. Actually, I wasn't
asking the question as I've been relatively worry free about it for some
time - unless a customer gets overly concerned about it.
I think Joe, and many others talk well about what it looks like and how it
compares with other such findings as hole wall pull away. I've been through
the well written 600 many times and can't even find anything concerning it.
For me, Section 3.1, and in particular 3.1.1's figure showing the thermal
and laminate evaluation zones and what falls out of it, pretty much tells
the whole story.
Earl
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|