Hi Stella! Just one bit of information to add to Steve's great information
- use the IPC JSTD-002A solderability specification as you tool/method of
demonstrating that the solderability and/or leaching is your problem. We
have experienced similar problems in the past and poor solderability of the
components was problem.
Dave Hillman
Rockwell Collins
[log in to unmask]
Stella Neyman <[log in to unmask]>@ipc.org> on 12/05/2001 05:53:55 PM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
To: [log in to unmask]
cc:
Subject: [TN] Platinum/Palladium/Silver plating
Dear technetts, Please help me out.
We are introducing new custom made SMT component: Medium size (approx. 0.5"
x 0.200") with 2 ceramic terminations that plated with Pt/Pd/Ag coating.
Solder paste for our reflow process is 63Sn/37Pb NC low residue. Reflow
profile is standard for this paste reflow peak temp of 220-225 deg C and 50
sec above 183 deg C.
We are experiencing non-wetting conditions on components terminations, some
solder joints cracked during thermocycling testing.
Does anybody experience problem with Pt/Pd/Ag coating over ceramic
substrate?
Any information would be greatly appreciated.
Sincerely
Stella Neyman
Jabil Circuit, MI
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|