Seyfi
My experience is that bridging with through-hole components is usually a
function of either doubtful solderability of the component lead and/or
PCB, the wrong chemistry or the poor curing of the solder mask (or
substrate, if there is no mask) - or a combination of any of these.
Solder thieves are usually used on the trailing edge of SMD components
(e.g., QFPs) to ensure that the break-off of the meniscus between the
solder wave and the solderable surface occurs away from the actual
connections, thereby reducing the risk of shorts between closely-spaced
leads. It will not cure bridging because of factors like poor
solderability. I've not heard of temporary thieving - isn't this called
borrowing? :-)
Brian
Seyfi Ozsever wrote:
>
> I am looking for some information in the market about "SOLDER THIEVES"
> that can be temporarily applied on the PCB's (i.e, can be removed after
> soldering) to prevent chronical solder bridge problems during wave
> soldering. Some through hole components and/or component leads are
> notorious for having the tendency of getting solder bridges at certain
> spots regardless of the adjustments in the process parameters.
>
> I would appreciate any suggestion or advise in this area.
>
> Thank you,
>
> Seyfi Ozsever
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|