Chuck,
Just as an FYI, it is not all that uncommon to use 100-150W Ar+ to clean
hybrids prior to wire bonding. Ditto for an O2 plama. We are not after
gross metal removal in that application - just cleaning of atomic scale
layer thicknesses.
Will leave the macroscopic surface treatment activities to you folks.
Steve Creswick - Gentex Corp
-----Original Message-----
From: Chuck Brummer [mailto:[log in to unmask]]
Sent: Tuesday, December 18, 2001 3:30 PM
To: [log in to unmask]
Subject: Re: [TN] Cleaning after plasma
Hi,
No, I'm not. (sorry)
Argon isn't going to etch epoxy or metal, and with only 100 watts is barely
going to clean
organics. Silicon is always tough. I like Rudy's suggestion (I usually do)
but if your going
to plasma use O2 with a dash (2%) of CF4 and crank up that power to like,
say, 1000 watts.
Chuck Brummer
Acuson
Good Luck!
[log in to unmask] wrote:
> Why do all that plasma cleaning of assemblies, dosen't plasma etch metal
and
> desmear epoxies, sounds like a lot of compoinents could be affected over
time.
> Could you just wash the bds. in a water spray sopinafer type machine?
>
>
----------------------------------------------------------------------------
-----
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
>
----------------------------------------------------------------------------
-----
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|