The damage laminate can be found in 600 under 2.2.3 Exposed/disrupted
Fibers. Exposed or disrupted fiber areas are considered conductive area and
if they reduce the minimum electrical spacing requirements, they are
nonconforming and must be repaired. IPC 6012, 3.3.2.2 Weave Exposure also
discussed the condition.
Hope this helps
Leo Lambert
EPTAC Corp
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Shawn Murphy
Sent: Monday, December 17, 2001 6:32 PM
To: [log in to unmask]
Subject: [TN] Trace cut quality
What specification would contain "Trace Cut" information? We have a
situation where there is obvious damage to the FR4 material between two
leads that had a common trace at one point. Our conscious tells us to
repair the gouge but we haven't located anything in IPC-610 to tell us what
is acceptable and what isn't. Any help would be greatly appreciated.
regards,
shawn
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|